FIller Metal Breakdown

S-NFC

Lorem ipsum dolor sit amet, consectetur adipiscing elit. Ut elit tellus, luctus nec ullamcorper mattis, pulvinar dapibus leo.

Classification

  • AWS A5.15/ASME SFA-5.15 ENiFe-CI
  • JIS Z 3252 DFCNiFe
  • EN ISO 1071 E C NiFe-CI 1
  • KS D7008 DGCNiFe

Approvals

Features

  • Good crack resistance
  • Preheat at 100~200°C (212~392°F)
  • Easy to remove slag

Application Areas

  • Welding of normal grades of cast iron

Base Materials to be welded

Welding process

  • Welding Positions: 1G 2F
  • Polarity: AC or DC ±
  • Redrying Conditions: 350°C (662°F) X 1hr

Diameter / Packaging

Diameter Length F&HF V-up/OH Packaging
2.6 (3/32) 300 (12) 55~80 PVC – Packet 2.5kg (5.5lbs), Carton 10kg (22lbs)
3.2 (1/8) 350 (14) 80~130 PVC – Packet 2.5kg (5.5lbs), Carton 10kg (22lbs)
4.0 (5/32) 350 (14) 110~160 PVC – Packet 2.5kg (5.5lbs), Carton 10kg (22lbs)
Diameter Length F&HF V-up/OH Packaging
2.6 (3/32) 300 (12) 55~80 PVC – Packet 2.5kg (5.5lbs), Carton 10kg (22lbs)
3.2 (1/8) 350 (14) 80~130 PVC – Packet 2.5kg (5.5lbs), Carton 10kg (22lbs)
4.0 (5/32) 350 (14) 110~160 PVC – Packet 2.5kg (5.5lbs), Carton 10kg (22lbs)

Typical Chemical Composition of the Wire (wt%)

C Si Mn P S Ni Fe
1.73 0.59 1.34 0.005 0.001 Bal. 45.7

Typical Mechanical Properties of All-Weld Meta

Hardness(HRB)
90

Contact Us Today